- Contact Person : Ms. Miao sumei
- Company Name : Zibo Taisheng Industry & Trade Co., Ltd.
- Tel : 86-533-3191633
- Fax : 86-533-3191016
- Address : Shandong,Zibo,Xilongjiao village, Kunlun Town, Zichuan district,
- Country/Region : China
- Zip : 255129
High Corrosion Resistance Boron Nitride Evaporation Boat For Non Ferrous Metal
(1)Standard:
110×16×9,110×20×10,105×20×10,120×24×10,110×26×10,130×30×10,110×30×10,130×35×10,150×35×10Can design other standards according to customers' requirements
(2) Physical performances:
1.Density:2.9-3.1g/cm^3 2.Resistivity:300-2000υΩ/cm3.Porosity:≤10%4.Thermal expansion coefficient :(4~6)×10-6cm/cm°C5.Temperature coefficient of resistance:(5~6)×10-4/°C6.Max working temperature :750°C
(3) Tehnology standard:1.Length:L±0.52.Width:B-0.13.Thickness:H±0.184.Bending strength:≤0.5mm5.Undersurface roughness :≤0.1mm6.Two sides nonparallelisn:≤0.2mm
(4)Using conditions:
1.working current:400-900A2.working voltage:5-15V3. working temperature:1300 - 1750°C4.evaporation rate:0.3-0.5g/ minute /cm^25. service life :10-15hours
(5)Properties of products:
1.Good thermal performance and good stability.
2.Good insulativity, Abrasion-resistance
3.Good processing performance, Precision can reach 0.01mm
4.Good chemistry stability,can not reaction with Metal And acid.
5.Pierce Infrared and microwave,absorption neutron
6.non-poisonous
(6)Application:
As melting aluminum and zinc sulfide, using in vacuum evaporation technology.
(7) Operating methods:
In order to play best capacity of evaporation boat, please operate as following:
1. Keep two rows of fixture alignment and keep the surface smooth.
2. When first heating for the new boat, please put an aluminium yarn in the central groove in order to judge the boat's temperature.
3. The connection point of Aluminium yarn should be located in 1/3 to 1/2 place of boat.
4. For the first heating for new boat, please don't heat quickly, in order to avoid to affecting air bleeding.
5. For the first time,the speed of sending aluminum should at the rate of 75% normal speed and increase gradually,And turn down the power in order to reach to max area of aluminum liquid.
6. For the first boat, first heating for 15 minutes will be best. And send aluminum to evaporate plating follow the above methods.
7. When each coil finished evaporating, please stop sending aluminium first. And stop the power 30-60 seconds later. Two minutes after stop power and the boat's color turn to dark red, than stop close vacuum.
High Corrosion Resistance Boron Nitride Evaporation Boat For Non Ferrous Metal